There are two major benefits for using the Amsoil Coolant Booster. (1) It can reduce engine temps up to 6 degrees when mixed with 50/50 antifreeze/water mixture and (2) it helps fight radiator corrosion.
The following information was taken from
http://www.amsoil.com/storefront/rdcb.aspx
Competitive testing comparing AMSOIL Dominator Coolant Boost and Red Line Water Wetter® was conducted in an independent laboratory. The ASTM corrosion tests featured in this study are designed to simulate the most grueling conditions cooling systems face, and are the actual test standards the automotive industry relies upon for the approval of engine coolant products.Test results show Dominator Coolant Boost provides enhanced temperature reduction and corrosion protection properties over Red Line Water Wetter.
To test temperature reduction capabilities, controlled engine dynamometer (dyno) tests were performed on a 350 cubic inch Chevy engine with an aluminum block and cylinder heads. In each phase of testing, the engine was operated at 4,500 rpm until coolant temperature stabilized. As benchmarks for the test, straight water coolant stabilized at 220°F and a 50/50 antifreeze/water mixture stabilized at 228°F.
Dominator Coolant Boost
Mixed with 50/50 Antifreeze/Water
6°F reduction
Mixed with Straight Water Coolant
19°F reduction
Red Line Water Wetter
Mixed with 50/50 Antifreeze/Water
3°F reduction
Mixed with Straight Water Coolant
12°F reduction
Cast Aluminum Alloys Corrosion Test
The Cast Aluminum Alloys Corrosion Test (ASTM D-4340) measures corrosion protection properties in modern automobile and high-performance race engines with aluminum cylinder heads. A cast aluminum puck was heated to 275°F at 28 PSI and exposed to the test coolant mixture for one week. Weight loss of less than 1.0 mg is required to pass the test.
Weight Loss in mg (1.00 max)
Dominator Coolant Boost
0.14
Weight Loss in mg (1.00 max)
Red Line Water Wetter
0.21
Weight Loss in mg (1.00 max)
Water Only
3.97
Corrosion Test in Glassware
In the Corrosion Test in Glassware (ASTM D-1384), six metal coupons constructed of the most common metals in automotive cooling systems were totally immersed in aerated coolant mixtures for 336 hours at 190°F. Each test was performed three times to determine the average weight change for each metal. The ASTM sets the “allowable” weight loss maximums for each metal.
Copper weight loss (mg), Allowable 10 max
Dominator Coolant Boost in straight water (1)
Red Line Water Wetter in straight water (1)
Water Only (25)
Solder weight loss (mg), Allowable 30 max
Dominator Coolant Boost in straight water (1)
Red Line Water Wetter in straight water (6)
Water Only (62)
Brass weight loss (mg), Allowable 10 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (2)
Water Only (23)
Steel weight loss (mg), Allowable 10 max
Dominator Coolant Boost in straight water (1)
Red Line Water Wetter in straight water (1)
Water Only (18)
Cast Iron weight loss (mg), Allowable 10 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (0)
Water Only (29)
Cast Aluminum weight loss (mg), Allowable 30 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (16)
Water Only (91)
Simulated Service Corrosion Test
In the Simulated Service Corrosion Test (ASTM D-2570), six metal coupons constructed of the most common metals in automotive cooling systems were exposed to ASTM corrosive water designed to simulate hard and corrosive water in degraded coolant for 1,064 hours at 190°F. Coolant was maintained at a temperature and flow rate equivalent to the operating conditions seen in most passenger vehicles. Corrosive weight loss suffered during the test determines the additive’s corrosion protection properties. The ASTM sets the “allowable” weight loss maximums for each metal.
Copper weight loss (mg), Allowable 20 max
Dominator Coolant Boost in straight water (7)
Red Line Water Wetter in straight water (6)
Water Only (66)
Solder weight loss (mg), Allowable 60 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (25)
Water Only (120)
Brass weight loss (mg), Allowable 20 max
Dominator Coolant Boost in straight water (3)
Red Line Water Wetter in straight water (5)
Water Only (59)
Steel weight loss (mg), Allowable 20 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (4)
Water Only (54)
Cast Iron weight loss (mg), Allowable 10 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (2)
Water Only (117)
Cast Aluminum weight loss (mg), Allowable 60 max
Dominator Coolant Boost in straight water (0)
Red Line Water Wetter in straight water (34)
Water Only (89)