Originally Posted by trippled View Post
We're you welding outside? Even a gentle breeze can blow your shielding gas away and give you porosity. Others aren't too bad tho. Mig spatter is pretty normal I'd say.
Yeah I was. Guess that would explain it then. I wasn't able to get a good pic of it but when doing the exhaust that was tricky. I think a large part was from welding upside down. I just couldn't get a good bead started. We also changed the spool to a smaller gauge wire and I don't think I had the welder set up right. We turned down the purge and wire speed but when I was upside down beads just did not like to stick.
__________________
88 MJ, 4.0, 4wd, 3 pedals, Shortbed.
Mods; ACOS, quick discos, HD tie rod and a bitchin air fresher
04 WJ, 4.7HO
Mods; 3" IRO lift, ADDCO rear sway bar, 4.7HO with bored fastman TB, AFE intake and Superchip tuner, 32s, lunchbox rear 242HD, 3" Kolak exhaust
Reply With Quote